Processing Properties Metric English Comments
Die Temperature 93.3 °C
200 °F
Extrusion
LG Chemical KEYFLEX TO-1045D Thermoplastic Olefin for Injection Molding, 45D Hardness
KEYFLEX resins, thermoplastic elastomers divided by polyester and polyolefin type, have been developed by LG`s own polymerization and compounding technology. They display the flexibility of rubber ..
Die Temperature 93.3 - 104 °C
200 - 220 °F
Blow molding
LG Chemical KEYFLEX TO-1045D Thermoplastic Olefin for Injection Molding, 45D Hardness
KEYFLEX resins, thermoplastic elastomers divided by polyester and polyolefin type, have been developed by LG`s own polymerization and compounding technology. They display the flexibility of rubber ..
Die Temperature 93.3 °C
200 °F
Extrusion
LG Chemical KEYFLEX TO-1075A Thermoplastic Olefin for Injection Molding, 75A Hardness
KEYFLEX resins, thermoplastic elastomers divided by polyester and polyolefin type, have been developed by LG`s own polymerization and compounding technology. They display the flexibility of rubber ..
Die Temperature 93.3 - 104 °C
200 - 220 °F
Blow molding
LG Chemical KEYFLEX TO-1075A Thermoplastic Olefin for Injection Molding, 75A Hardness
KEYFLEX resins, thermoplastic elastomers divided by polyester and polyolefin type, have been developed by LG`s own polymerization and compounding technology. They display the flexibility of rubber ..
Die Temperature 93.3 °C
200 °F
Extrusion
LG Chemical KEYFLEX TO-1088A Thermoplastic Olefin for Injection Molding, 88A Hardness
KEYFLEX resins, thermoplastic elastomers divided by polyester and polyolefin type, have been developed by LG`s own polymerization and compounding technology. They display the flexibility of rubber ..
Die Temperature 93.3 - 104 °C
200 - 220 °F
Blow molding
LG Chemical KEYFLEX TO-1088A Thermoplastic Olefin for Injection Molding, 88A Hardness
KEYFLEX resins, thermoplastic elastomers divided by polyester and polyolefin type, have been developed by LG`s own polymerization and compounding technology. They display the flexibility of rubber ..
Die Temperature 93.3 °C
200 °F
Extrusion
LG Chemical KEYFLEX TO-1175A Thermoplastic Olefin for Extrusion, 75A Hardness
KEYFLEX resins, thermoplastic elastomers divided by polyester and polyolefin type, have been developed by LG`s own polymerization and compounding technology. They display the flexibility of rubber ..
Die Temperature 93.3 - 104 °C
200 - 220 °F
Blow molding
LG Chemical KEYFLEX TO-1175A Thermoplastic Olefin for Extrusion, 75A Hardness
KEYFLEX resins, thermoplastic elastomers divided by polyester and polyolefin type, have been developed by LG`s own polymerization and compounding technology. They display the flexibility of rubber ..
Die Temperature 93.3 °C
200 °F
D5
Kostat E-3007J Conductive PS Compound
KOSTAT E-3007J is a conductive thermoplastic compound based on impact modified polystyrene and a special conductive carbon black.KOSTAT E-3007J is not dependant on atmospheric conditions.Special Fea..
Die Temperature 93.3 °C
200 °F
D1
Kostat E-3007J Conductive PS Compound
KOSTAT E-3007J is a conductive thermoplastic compound based on impact modified polystyrene and a special conductive carbon black.KOSTAT E-3007J is not dependant on atmospheric conditions.Special Fea..