Processing Properties | Metric | English | Comments |
---|---|---|---|
Die Temperature | 87.8 °C | 190 °F | D3 |
Kostat E-3007J Conductive PS Compound KOSTAT E-3007J is a conductive thermoplastic compound based on impact modified polystyrene and a special conductive carbon black.KOSTAT E-3007J is not dependant on atmospheric conditions.Special Fea.. |