Polymer Property : Die Temperature = 653 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Die Temperature 345 - 365 °C
653 - 689 °F
Lubrizol Advanced Materials PEARLCOAT® 165K Thermoplastic Polyurethane Elastomer
PEARLCOAT® 165K is a polyether based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent low-temperature flexibility and very good hydrolysis resistance. PE..