Processing Properties | Metric | English | Comments |
---|---|---|---|
Die Temperature | 249 °C | 480 °F | Die Zone 2 |
SK Chemicals SKYGREEN® PETG 2008 Specially Formulated PET Copolymer Resin SKYGREEN PETG is an amorphous copolyester in which a certain amount of ethylene glycol is replaced with 1,4-cyclohexane dimethanol (CHDM), which prevent crystallization, leading to improved processa.. |