Processing Properties | Metric | English | Comments |
---|---|---|---|
Die Temperature | 193 - 204 °C | 380 - 400 °F | Extrusion |
Laurel BioComposite Bio-Resâ„¢ 20% Composite in HDPE Bio-Resâ„¢ can be blended with various resins in certain applications. It can be included at rates up to 40% in manufactured plastic products while maintaining or enhancing the desired characteri.. |