Processing Properties | Metric | English | Comments |
---|---|---|---|
Die Temperature | 195 - 293 °C | 383 - 560 °F | Average value: 254 °C Grade Count:5 |
Overview of materials for PETG Copolyester This property data is a summary of similar materials in the MatWeb database for the category "PETG Copolyester". Each property range of values reported is minimum and maximum values of appropriate M.. |