Processing Properties | Metric | English | Comments |
---|---|---|---|
Die Temperature | 120 °C | 248 °F | |
Borealis LE0520 Polyethylene Compound, Crosslinkable, Semiconductive LE0520 is a Strippable Semi conductive Insulation Shielding for Power Cables. LE0520 is suitable for use in triple extrusion processes. Strip forces in the range of 3-6 kN/m (7-14 lbs/half inch) ha.. |
|||
Die Temperature | >= 120 °C | >= 248 °F | |
Borealis Low Sulfur™ LE0594 Crosslinkable Semiconductive Compound for Shielding of Power Cables Low Sulphur LE0594 is designed for use as a conductor and bonded insulation shield for medium and high voltage cables. LE0594 is a peroxide crosslinkable compound and is specifically intended to me.. |
|||
Die Temperature | >= 120 °C | >= 248 °F | |
Borealis Low Sulfur™ LE0595 Crosslinkable Semiconductive Compound for Shielding of Power Cables Low Sulphur LE0595 is designed for use as a conductor and bonded insulation shield for medium and high voltage cables. LE0594 is a peroxide crosslinkable compound and is specifically intended to me.. |