Processing Properties Metric English Comments
Die Temperature 202 °C
396 °F
Extrusion
Alliance Polymers Zythane™ 7075A Thermoplastic Polyurethane Elastomer
Zythane™ 7075A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Die Temperature 202 °C
396 °F
Zone 1, 6, Extrusion
Lubrizol ESTANE® 58211 Ether Based Thermoplastic Polyurethane
Features: Halogenated flame retardant compound – High hardnessUses: Extrusion – wire and cable jacketing and general extrusion where flame retardant propertied are requiredAvailable in Americas, E..