Processing Properties | Metric | English | Comments |
---|---|---|---|
Die Temperature | 198 °C | 388 °F | Extrusion |
Alliance Polymers Zythane™ 7070A Thermoplastic Polyurethane Elastomer Zythane™ 7070A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |