Processing Properties Metric English Comments
Adapter Temperature 150 °C
302 °F
Extrusion
Huntsman IROGRAN® PS455-200 TPU-Polyester
Introduction: IROGRAN PS455-200 is a polyester based thermoplastic polyurethane intended for extrusion applications. IROGRAN PS455-200 is part of the HUNTSMAN film and sheet product range and offers..