Processing Properties Metric English Comments
Adapter Temperature 213 °C
415 °F
5, Extrusion
Lubrizol Estane® ETE 55DS3 Thermoplastic Polyurethane, Easy-to-Extrude
Type: Estane® ETE 55DS3 is a 55D aromatic polyester-based thermoplastic polyurethane (TPU).Features: Hard TPU with wide extrusion processing window and melt stability, low temperature flexibility, ..
Adapter Temperature 213 °C
415 °F
5, Extrusion
Lubrizol ESTANE® ETE60DS3 Ester Based Thermoplastic Polyurethane
Features: Hard TPU with wide extrusion processing window and melt stability, high transparencyUses: Extrusion: Hose and Tube, Extrusion: Profile, Cable Jacket; Injection molding: VariousAvailable in..