Polymer Property : Feed Temperature = 464 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Feed Temperature 235 - 240 °C
455 - 464 °F
Solvay TECHNYL® A 52 G1 MX 20 PA66, Eh 0
Description: TECHNYL A 52 G1 MX20 is a Polyamide 6.6 glow wire resistant, reinforced with mineral fillerColors: it is marketed in black color.Available in: Latin AmericaMain Properties: ?Glow wire r..
Feed Temperature 220 - 240 °C
428 - 464 °F
Borealis Nepol™ GB601HP Polypropylene, 40% Long Glass Fiber Reinforced w/HK060AE
Nepol™ GB601HP is a special long glass fiber reinforced polypropylene concentrate grade intended for injection molding and extrusion. This material is designed for the dilution process in combinat..