Processing Properties | Metric | English | Comments |
---|---|---|---|
Feed Temperature | 193 °C | 380 °F | |
Lubrizol Advanced Materials PEARLTHANE® 16N87 Thermoplastic Polyurethane Elastomer
(discontinued **) PEARLTHANE® D16N87 is a polyether-based TPU, supplied in form of translucent, colourless or slightly yellowish pellets, offering adequate hardness with superior hydrolysis resistance and improved e.. |
|||
Feed Temperature | 193 °C | 380 °F | |
Lubrizol Advanced Materials PEARLTHANE® 16N92 Thermoplastic Polyurethane Elastomer
(discontinued **) PEARLTHANE® 16N92 is a polyether based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent mechanical properties and excellent hydrolysis resistance. It can b.. |
|||
Feed Temperature | 193 °C | 380 °F | |
Lubrizol Advanced Materials PEARLTHANE® 11T85UV Thermoplastic Polyurethane Elastomer PEARLTHANE® 11T85UV is a UV resistant polycaprolactone copolyester based TPU, supplied in form of translucent, colourless or slightly yellowish pellets, featuring adequate hardness with excellent.. |