Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 4-x | 135 - 141 °C | 275 - 285 °F | |
LyondellBasell Petrothene® YR19548 Polyolefin Compound ApplicationsPETROTHENE YR 19548 is a colorable, thermoplastic non-halogenated, flame retardant polyolefin compound formulated for small gauge automotive primary insulation (SAE J1128) and appliance .. |