Processing Properties | Metric | English | Comments |
---|---|---|---|
Cycle Time - Injection | 3.7 sec | 3.7 sec | |
Lubrizol Advanced Materials PEARLTHANE® 16N92 Thermoplastic Polyurethane Elastomer
(discontinued **) PEARLTHANE® 16N92 is a polyether based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent mechanical properties and excellent hydrolysis resistance. It can b.. |