Processing Properties | Metric | English | Comments |
---|---|---|---|
Cycle Time - Injection | 2.5 sec | 2.5 sec | |
Lubrizol Advanced Materials PEARLTHANE® 16N87 Thermoplastic Polyurethane Elastomer
(discontinued **) PEARLTHANE® D16N87 is a polyether-based TPU, supplied in form of translucent, colourless or slightly yellowish pellets, offering adequate hardness with superior hydrolysis resistance and improved e.. |
|||
Cycle Time - Injection | 2.5 sec | 2.5 sec | |
Lubrizol Advanced Materials PEARLTHANE® 15N95UV Thermoplastic Polyurethane Elastomer PEARLTHANE® 15N95UV is a polyether copolymer-based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent mechanical properties and excellent hydrolysis resist.. |