Processing Properties | Metric | English | Comments |
---|---|---|---|
Drying Temperature | 37.8 - 48.9 °C @Time 14400 - 18000 sec |
100 - 120 °F @Time 4.00 - 5.00 hour |
out of open box |
Green Dot Terratek® Flex GDH-B1 Compostable Bioplastic Elastomer GDH-B1 is an elastomeric bioplastic with a diverse range of potential applications. It is a starch-based elastomer that is strong, durable and pliable with an exquisite soft touch. The bioplastic i.. |