Polymer Property : Pot Life = 9.0 min Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Pot Life 9.0 - 11 min
9.0 - 11 min
100 gram mass
Master Bond EP21LSCL-1 Two Component, Room Temperature Curing Epoxy Resin
Product Description: Master Bond Polymer System EP21LSCL-1 is a two component, low viscosity epoxy resin system featuring optical clarity as well as non-yellowing properties. This system can be used..