Processing Properties Metric English Comments
Pot Life 60 - 85 min
60 - 85 min
200 gram mass
Master Bond EP21LV35Med Two Component, Flexible USP Class VI Epoxy System
Master Bond Polymer System EP21LV3/5Med is a two part, low viscosity epoxy resin system for high performance bonding, sealing, coating, encapsulation and casting that cures flexible. It cures readil..