Processing Properties | Metric | English | Comments |
---|---|---|---|
Pot Life | 80.0 min @Temperature 25.0 °C |
80.0 min @Temperature 77.0 °F |
100 grams |
Cytec (Conap) FR-1047 / EA-028 Conapoxy® Resin / Conacure® Hardener Epoxy Potting and Encapsulating Systems for Electronic ApplicationsHigh technology epoxy resin systems for potting and encapsulation, for the defense, aerospace, electronics, computer, automotive an.. |