Processing Properties | Metric | English | Comments |
---|---|---|---|
Pot Life | 70.0 min @Temperature 25.0 °C |
70.0 min @Temperature 77.0 °F |
0.5 lbm |
Cytec EN-9 (Conap) Casting, Potting, and Molding Compound High Technology Potting, Casting and Molding CompoundsTwo-component, polybutadiene-based liquid urethane casting and potting systems. When reacted these high technology systems produce tough, stable.. |
|||
Pot Life | 70.0 min @Temperature 25.0 °C |
70.0 min @Temperature 77.0 °F |
0.5 lbm |
Cytec EN-9 (OZR) (Conap) Casting, Potting, and Molding Compound High Technology Potting, Casting and Molding CompoundsTwo-component, polybutadiene-based liquid urethane casting and potting systems. When reacted these high technology systems produce tough, stable.. |