Processing Properties | Metric | English | Comments |
---|---|---|---|
Pot Life | <= 6.00 min @Temperature 25.0 °C |
<= 6.00 min @Temperature 77.0 °F |
100 g |
Armstrong X-81/A Epoxy Adhesive Information provided by Ellsworth Adhesives. |
|||
Pot Life | <= 6.00 min @Temperature 25.0 °C |
<= 6.00 min @Temperature 77.0 °F |
100 g |
Armstrong X-81-A/F Epoxy Adhesive Information provided by Ellsworth Adhesives. |
|||
Pot Life | 6.00 min | 6.00 min | uncured |
Atom Adhesives AA-DUCT 905 Epoxy Adhesive AA-DUCT 905 is a single component epoxy, formulated with pure silver powder combined with organic binders and solvents to produce electrically conductive paths, films or patterns over non-conductive.. |