Processing Properties | Metric | English | Comments |
---|---|---|---|
Pot Life | 58.0 min @Temperature 23.9 °C |
58.0 min @Temperature 75.0 °F |
|
ITW Devcon Metal Repair Stainless Steel Putty (ST), Grey Information provided by ITW Devcon |