Processing Properties Metric English Comments
Pot Life 56.0 min

@Temperature 23.9 °C
56.0 min

@Temperature 75.0 °F
Devcon High-Performance Backing Compound Epoxy
Abrasion-Resistant SystemData provided by Ellsworth Adhesives.