Processing Properties | Metric | English | Comments |
---|---|---|---|
Pot Life | 55 min @Temperature 24.0 °C |
55 min @Temperature 75.2 °F |
|
BCC Products BC 5105 Epoxy Laminating System BC 5105 is a clear, unfilled, low viscosity laminating system. This heat resistant resin exhibits excellent wet out, reasonable working time and may be used at room temperature without post-curing. .. |
|||
Pot Life | 55 - 60 min @Temperature 24.0 °C |
55 - 60 min @Temperature 75.2 °F |
1 lb. mass |
BCC Products BC 7053 Epoxy Casting BC 7053 is an iron filled epoxy casting system. This system is a high iron content material that provides unsurpassed wear resistance. BC7053 was designed for use in constructing core boxes, holding.. |