Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Pot Life 24 min
24 min
Huntsman Euredur 43 S Cycloaliphatic Amine
Approx. H+ equivalent weight 115. Mix Ratio with GY 6010 is 60.Comments/Applications: Euredur 43 S is the accelerated version of Euredur 43.Data provided by Ciba Specialty Chemicals.Ciba Specialty..
Pot Life 24 min
24 min
Huntsman HZ 815 X-70 US Aromatic Amine
Approx. H+ equivalent weight 150. Mix Ratio with GY 6010 is 81.Comments/Applications: Solution of HY 815, 70% solids in xylene. Trade sale paint enamels. Industrial maintenance, FDA. Flexible m..