Processing Properties | Metric | English | Comments |
---|---|---|---|
Pot Life | 21 min | 21 min | |
Huntsman Euredur 14 Cycloaliphatic Amine Approx. H+ equivalent weight 75. Mix Ratio with GY 6010 is 40.Comments/Applications: Mannich based low viscosity, highly reactive hardener to be used on humid surfaces, epoxy mortars in solvent fr.. |