Processing Properties | Metric | English | Comments |
---|---|---|---|
Pot Life | 2.5 min | 2.5 min | |
Taiwan PU Corporation PPG CPU-2172 Polyurethane Casting Elastomer A urethane elastomer that can be cured by reacting with a polyamine or a polyolhardener. The molding process is composed of pre-heating, degassing, maxing with a hardener, pouring into the mold, cu.. |
|||
Pot Life | 2.5 min | 2.5 min | |
Taiwan PU Corporation PTMG CPU-325L Polyurethane Casting Elastomer A urethane elastomer that can be cured by reacting with a polyamine or a polyolhardener. The molding process is composed of pre-heating, degassing, maxing with a hardener, pouring into the mold, cu.. |
|||
Pot Life | 2.5 - 3.0 min | 2.5 - 3.0 min | 100 gram mass |
Master Bond EP30DPMed USP Class VI, Two Component Epoxy Urethane System Master Bond Polymer System EP30DPMED is a versatile, two component, epoxy-urethane elastomeric compound, featuring superior strength, toughness, and abrasion resistance for high performance bonding,.. |