Processing Properties | Metric | English | Comments |
---|---|---|---|
Pot Life | 0.0833 - 1.00 min | 0.0833 - 1.00 min | Average value: 0.449 min Grade Count:29 |
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade". Each property range of values reported .. |