Polymer Property : Pot Life = 0.75 min Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Pot Life 0.75 min
0.75 min
Open Time
Valley Adhesives EM-490 High Temperature Application Glue Stick
Valley Adhesives EM-490 High Temperature Application Glue StickExcellent tack; Used on plastics, metals and other surfaces.
Pot Life 0.75 min
0.75 min
Open Time
Valley Adhesives EM-600 High Temperature Application Glue Stick
Valley Adhesives EM-600 High Temperature Application Glue StickBonds many woods and wood composites; Excellent for woodworking and cabinetry.
Pot Life 0.75 min
0.75 min
Open Time
Valley Adhesives EM-115 High Performance Application Glue Stick
Valley Adhesives EM-115 High Performance Application Glue StickHigh peel, shear strength, and heat resistance; Good wetting and heat resistance for potting; Excellent adhesion to wood, plastics, pol..