Processing Properties | Metric | English | Comments |
---|---|---|---|
Pot Life | 0.670 min | 0.670 min | |
Northstar Polymers FFM-1 Firm-Grade Flexible Open-Cell Foam This foam formulation is particularly designed to make flexible but firm open-cell foam by either hand-mixing or machine casting. This material may be suitable for products that require some load b.. |
|||
Pot Life | 0.670 - 0.840 min | 0.670 - 0.840 min | |
Northstar Polymers MPP-R07B Polyurethane Formulation This foam polyurethane formulation is designed yield structural foam by either hand-mixing or machine casting method. The pot-life of this material is long enough to allow manual handling for cast-.. |