Polymer Property : Pot Life = 0.58 min Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Pot Life 0.58 min
0.58 min
Open Time
Valley Adhesives EM-420 High Temperature Application Glue Stick
Valley Adhesives EM-420 High Temperature Application Glue StickBonds many plastics, polyolefins and light weight materials.