Polymer Property : Pot Life = 0.20 min Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Pot Life 0.15 - 0.20 min
0.15 - 0.20 min
Open Time
Bostik 6332 Quick Setup EVA Glue Stick
Bostik 6332 Quick Setup EVA Glue StickShort open time and quick set up. Low viscosity. Easy to gun. Withstands elevated temperatures.