Processing Properties | Metric | English | Comments |
---|---|---|---|
Pot Life | 0.170 - 0.250 min | 0.170 - 0.250 min | |
Northstar Polymers MPS-F04A Hand-Mixable Flexible Foam This foam formulation is designed to make molded flexible foam parts/sheets/dies/blocks by hand-mixing or by the meter dispensing equipment. The components are stable liquid at room temperature and.. |