Processing Properties | Metric | English | Comments |
---|---|---|---|
Head Temperature | 175 - 215 °C | 347 - 419 °F | Blow Molding |
LG Chemical HYPERIER IP1306B PA-HDPE Nanoclay Compound HYPERIER is a nano compound made from nano-sized inorganic plate clay. Blow Molding, Barrier thermoplastic, Nylon blend with HDPEApplication: Agrochemical Container, SORE* Fuel Tank, PFCCAS No. 900.. |