Processing Properties | Metric | English | Comments |
---|---|---|---|
Head Temperature | 130 - 150 °C | 266 - 302 °F | |
Fainplast Compounds HAX HFX 024-15C Halogen Free PVC This product is a LSFOH silane grafted compound for cable insulation and sheating, cross-linkable by heat and moisture by previous addition of a suitable catalyst masterbatch. It is recommended to s.. |
|||
Head Temperature | 130 - 150 °C | 266 - 302 °F | |
Fainplast Compounds HAX HFX 024-21L Halogen Free PVC This product is a LSFOH silane grafted compound for cable insulation and sheating, cross-linking by heat and moisture by previous addition of a suitable catalyst masterbatch. It is highly recommende.. |
|||
Head Temperature | 130 - 165 °C | 266 - 329 °F | Average value: 146 °C Grade Count:3 |
Overview of materials for PVC, Wire and Cable Grade This property data is a summary of similar materials in the MatWeb database for the category "PVC, Wire and Cable Grade". Each property range of values reported is minimum and maximum values of appr.. |