Hot-Working Temperature 749 - 1200 °C
1380 - 2190 °F
Uniformly heating
Schmolz + Bickenbach UgiPermâ„¢ 12FM Stainless Steel Bar
Description: UgiPermâ„¢ 12FM is a 12% chrome ferritic stainless with improved magnetic properties designed for use in electro-injectors, valves and many other applications. The grade was develope..