Processing Properties | Metric | English | Comments |
---|---|---|---|
Hot-Working Temperature | >= 949 °C | >= 1740 °F | Forge |
Schmolz + Bickenbach UGIMA® 316/316L Stainless Steel Bar Description: 316/316L UGIMA® is Ugitech’s improved machining grade produced only by Ugitech. It is identical in every way to regular 316L, except with respect to machinability. 316/316L UGIM.. |
|||
Hot-Working Temperature | 949 - 1200 °C | 1740 - 2190 °F | Forging range |
Schmolz + Bickenbach UGIMA® 630 Stainless Steel Bar Description: 630 UGIMA® is an improved machining martensitic precipitation hardenable grade produced only by Ugitech. It is identical in every way to standard type 630 (17-4), except with respect.. |