Polymer Property : Hot-Working Temperature = 1382 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Hot-Working Temperature 750.0 - 1200 °C
1382 - 2192 °F
Uniformly heating
Schmolz + Bickenbach 430FR Stainless Steel Bar
Description: Ugitech’s 430FR is a ferritic stainless steel designed for soft magnetic components operating in corrosive environments. The 17.00% - 18.00% chromium makes corrosion resistance sim..
Hot-Working Temperature 750.0 - 1200 °C
1382 - 2192 °F
Uniformly heating
Schmolz + Bickenbach IMRE™ Stainless Steel Bar
Description: Ugine IMRE™ is a chromium stainless steel with improved magnetic properties used in solenoid valves. IMRE™ is at 18% chromium ferritic stainless steel with 2% Mo designed to withstand..