Processing Properties | Metric | English | Comments |
---|---|---|---|
Die Cooling Temperature | 200 - 240 °C | 392 - 464 °F | |
Solvay Specialty Polymers Polidiemme® G/220 Thermoset Elastomer (TSE) Polidiemme® XLPO -Cross-linkable Polyolefin. Elastomer based compound crosslinkable by ambient moisture, consisting of a silane pregrafted base compound to be used with a catalyst masterbatch (S.. |