Processing Properties Metric English Comments
Die Cooling Temperature 170 - 220 °C
338 - 428 °F
Solvay Specialty Polymers Cogegum® GFR/340 Polyolefin
Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound. Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a poly..
Die Cooling Temperature 170 - 220 °C
338 - 428 °F
Solvay Specialty Polymers Cogegum® GFR/340-HP Polyolefin
Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound. Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a poly..