Processing Properties Metric English Comments
Die Opening 0.0760 - 0.280 cm
0.0299 - 0.110 in
Average value: 0.164 cm Grade Count:8
Overview of materials for High Density Polyethylene (HDPE), Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Film Grade". Each property range of values reported is minimum and max..
Die Opening 0.0760 - 0.130 cm
0.0299 - 0.0512 in
Chevron Phillips MarFlex® 9656 HDPE Blown Film Resin
Resin Type: high density, linear polyethylene.Characteristics: copolymerization enhances film toughness, good drawdown, density level gives good machinability, blend well with LLDPEApplications: not..
Copyright © lookpolymers.com All Rights Reserved