Vent Depth 0.00127 - 0.00203 cm
0.000500 - 0.000800 in
MRC Polymers NAXALOYâ„¢ 780 GF11 PC+PBT Polyester Blend, 11% Glass Fiber Filled
Good chemical resistance, impact and heat resistanceAvailable in Black OnlyCan be UV StabilizedInternal and external lubricant can be added.Information provided by MRC Polymers Inc.
Vent Depth 0.00127 - 0.00203 cm
0.000500 - 0.000800 in
MRC Polymers NAXALOYâ„¢ 780 PC+PBT Polyester Blend
Good chemical resistance, impact and heat resistance.Information provided by MRC Polymers Inc.