Injection Pressure 68.5 - 107.7 MPa
9940 - 15620 psi
Samsung Cheil Industries TRANEX® TX-0520T Transparent Grade ABS
Information provided by Polymer Technology and Services, LLC (PTS).
Injection Pressure 68.5 - 107.7 MPa
9940 - 15620 psi
Samsung Cheil Industries TRANEX® TX-0520T Transparent Grade ABS
Information provided by Polymer Technology and Services, LLC (PTS).