Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Injection Pressure = 69.6 MPa Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Injection Pressure 40.0 - 69.6 MPa
5800 - 10100 psi
Premix Thermoplastics PRE-ELEC® CP 1318  (discontinued **)
PRE-ELEC CP 1318 is a conductive thermoplastic compound based on a polyolefin copolymer. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivit..
Copyright © lookpolymers.com All Rights Reserved