Polymer Property : Injection Pressure = 6000 psi
Polymer Property :
Injection Pressure =
6000 psi
Product List
Processing Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties
Metric
English
Comments
Injection Pressure
33.1
-
41.4
MPa
4800
-
6000
psi
Secondary
Clariant Renol PCSP0019 Polycarbonate/Acrylic Alloy
Data provided by Clariant Masterbatches