Processing Properties | Metric | English | Comments |
---|---|---|---|
Injection Pressure | 140 MPa | 20300 psi | |
Beijing Chemical Industry KAIFA® M109-G20 MPPO Resin 20% glass fiber reinforcedInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Injection Pressure | 140 MPa | 20300 psi | |
Beijing Chemical Industry KAIFA® M109-G20N MPPO Resin 20% glass fiber reinforced, flame retardantInformation provided by Beijing Chemical Industry Research Institute (Group) |