Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Injection Pressure = 1800 psi Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Injection Pressure 5.52 - 12.4 MPa
800 - 1800 psi
Ravago Manufacturing Americas Hybrid S464LGUV Acrylonitrile Butadiene Styrene + PC Alloy
Available in North America UV Stabilizer Good Toughness Low Gloss RoHS Compliant Form: Pellets Processing Method: Injection Molding Automotive Specifications: Chrysler MS-DB300 CPN4352 Color:..
Injection Pressure 6.89 - 12.4 MPa
1000 - 1800 psi
Ravago Manufacturing Americas Hylex® P1010LLT Polycarbonate
Information provided by Ravago.
Injection Pressure 6.21 - 12.4 MPa
900 - 1800 psi
Ravago Manufacturing Americas Hylex® P1018LLT Polycarbonate
Information provided by Ravago.
Injection Pressure 6.89 - 12.4 MPa
1000 - 1800 psi
Ravago Manufacturing Americas Hylex® P1310LLT Polycarbonate
Information provided by Ravago
Injection Pressure 6.21 - 12.4 MPa
900 - 1800 psi
Ravago Manufacturing Americas Hylex® P1318LLT Polycarbonate
Information provided by Ravago.
Injection Pressure 5.52 - 12.4 MPa
800 - 1800 psi
Ravago Manufacturing Americas Hybrid S464LG Acrylonitrile Butadiene Styrene + PC Alloy
Available in North America Good Toughness Low Gloss RoHS Compliant Form: Pellets Processing Method: Injection Molding Automotive Specifications: Chrysler MS-DB300 CPN4352 Color: Natural, Chry..
Injection Pressure 5.52 - 12.4 MPa
800 - 1800 psi
Ravago Manufacturing Americas Hylex® P1325L Polycarbonate, UV Stabilized, High Flow, Mold Release
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente..
Injection Pressure 6.21 - 12.4 MPa
900 - 1800 psi
Entec Hylex® P1017FR Polycarbonate
Information provided by Ravago.
Injection Pressure 6.89 - 12.4 MPa
1000 - 1800 psi
Entec Hylex® P1310FR Polycarbonate
Information provided by Ravago
Injection Pressure 6.21 - 12.4 MPa
900 - 1800 psi
Entec Hylex® P1317FR Polycarbonate
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente..
Injection Pressure 6.89 - 12.4 MPa
1000 - 1800 psi
Entec Hylex® P1010FR Polycarbonate
Information provided by Ravago.