Processing Properties | Metric | English | Comments |
---|---|---|---|
Injection Pressure | 10.3 - 13.8 MPa | 1500 - 2000 psi | |
Ravago Manufacturing Americas Hylex® P1007L Polycarbonate Information provided by Ravago |
|||
Injection Pressure | 10.3 - 13.8 MPa | 1500 - 2000 psi | |
Ravago Manufacturing Americas Hylex® P1307L Polycarbonate Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente.. |