Processing Properties | Metric | English | Comments |
---|---|---|---|
Injection Pressure | 5.90 - 7.90 MPa | 856 - 1150 psi | |
Samyang Triel® 5400 Thermoplastic Polyether Ester Elastomer TRIEL® resins offer superior mechanical properties, elasticities, heat and chemical resistance, which allow it to be widely used for electric/electronic equipments, automotive parts and outdoor r.. |
|||
Injection Pressure | 5.90 - 7.90 MPa | 856 - 1150 psi | |
Samyang Triel® 5407EF Thermoplastic Polyether Ester Elastomer TRIEL® resins offer superior mechanical properties, elasticities, heat and chemical resistance, which allow it to be widely used for electric/electronic equipments, automotive parts and outdoor r.. |
|||
Injection Pressure | 5.90 - 7.90 MPa | 856 - 1150 psi | Average value: 6.90 MPa Grade Count:18 |
Overview of materials for Polyether Ester Elastomer This property data is a summary of similar materials in the MatWeb database for the category "Polyether Ester Elastomer". Each property range of values reported is minimum and maximum values of appr.. |
|||
Injection Pressure | 5.90 - 7.90 MPa | 856 - 1150 psi | |
Samyang Triel® 5300 Thermoplastic Polyether Ester Elastomer TRIEL® resins offer superior mechanical properties, elasticities, heat and chemical resistance, which allow it to be widely used for electric/electronic equipments, automotive parts and outdoor rec.. |